基于M积分与实测载荷谱的转向架构架缺陷尺寸安全评估

  • 摘要: 为评估不同缺陷条件下转向架构架的裂纹驱动力,本文选取某型号转向架构架为对象,建立三维有限元模型,并在导柱定位座与侧梁圆角焊趾处通过Franc 3D植入不同尺寸的半椭圆表面裂纹。基于实测线路载荷谱的等效输入,采用M积分方法提取裂纹前缘I型应力强度因子( K_I )的分布,分析缺陷尺寸对应力强度因子的影响,并与材料门槛值进行对照。结果表明,所考察的4组初始裂纹中,最大 K_I 分别约为10.58、9.88、6.41和4.69 MPa·m1/2;与ZG230-450材料门槛值5.9 MPa·m1/2对比,前三组更易满足扩展起始条件,而第4组低于门槛值。研究形成了基于“缺陷尺寸— K_I 分布—门槛对照”的评估流程,可为在役构架的裂纹筛查、检修阈值设定及后续裂纹增长与寿命分析提供参数参考。

     

    Abstract: To assess the crack driving force of bogie frames under different defect conditions, this study selected a specific type of bogie frame as the research object and established a three-dimensional finite element model. Semi-elliptical surface cracks of varying sizes were introduced at the fillet weld toes between the guide pillar positioning seats and side beams using Franc 3D. Based on the equivalent input of measured track load spectra, the M-integral method was adopted to extract the distribution of Mode I stress intensity factor ( K_I ) along the crack front. The influence of defect size on the stress intensity factor was analyzed, with the results further compared against the material threshold value.The findings indicate that among the four groups of initial cracks investigated, the maximum K_I values were approximately 10.58, 9.88, 6.41 and 4.69 MPa·m1/2, respectively. When compared with the threshold value of 5.9 MPa·m1/2 for ZG230-450 steel, the first three groups were more likely to meet the crack propagation initiation criteria, while the fourth group remained below the threshold. This research establishes an evaluation framework based on the “defect size- K_I distribution-threshold comparison” paradigm. It can provide parametric references for crack inspection of in-service bogie frames, determination of maintenance thresholds, and subsequent analysis of crack growth and service life.

     

/

返回文章
返回